摘要 塔里木盆地台盆区自喷井完井投产管柱多使用常闭阀,目前现场使用的常闭阀存在可靠性低等不足之处,技术人员创新研制出了新型双通道常闭阀,该新型阀打开后能够实现管柱内外、上下同时沟通,解决了老式常闭阀可靠性低、不能对下部井筒压井等问题.提高了现场施工井控安全,该新型阀现场推广应用10余井次,成功率100%,应用效果好,现已在塔里木盆地完井试油中推广应用。 Normally-closed valves are often used in the production string of well completion in the flowing wells in the Taipeng area of Tarim basin.Due to the low reliability of the normally-closed valve used at well site,a new type of dual-channel normally-closed valve has been developed by the technicians,which can simultaneously communicate both inside and outside or both top and bottom of the string after opening,so as to deal with the problems such as the low reliability of the old type normally-closed valve and failure to kill a well at the lower wellbore and to improve the site operation safety of well control.The new valves have been widely used in more than 10 wells,with a success rate of 100%and a good application effect,which have been widely applied in the well testing of Tarim basin.
作者 严德荣 YAN Derong(Downhole Testing Company of Sinopec Oilfield Service Jianghan Corporation,Wuhan,Hubei,430040,China)
出处 《江汉石油职工大学学报》 2020年第6期60-62,共3页 Journal of Jianghan Petroleum University of Staff and Workers
关键词 塔里木盆地 双通道常闭阀 完井投产 Tarim Basin Dual—Channel Normally-Closed Valve Completion and Put into Production
  • 相关文献

参考文献2

二级参考文献8

  • 1吕拴录,赵国仙,王新虎,严密林,付道明,张建新.特殊螺纹接头油管腐蚀原因分析[J].腐蚀与防护,2005,26(4):179-181. 被引量:37
  • 2Lu S L,Zhang G Z,Lu M X. Analysis of N80 BTC Downhole Tubing Corrosio[J].Materials Performance,2004,(10):35.
  • 3Waite J P,Nesic S. Erosion in Disturbed Liquid/Particle Pipe Flow:Effects of Flow Geometry and Particle Surface Roughness[J].Corrosion,1993,(10):850.doi:10.5006/1.3316009.
  • 4Levy A V. Erosion-Corrosion of Metals[J].Corrosion,1995,(11):872.doi:10.5006/1.3293564.
  • 5Waite J P,Nesic S. Erosion in Disturbed Liquid/Particle Pipe Flow:effects of flow geometry and particle surface roughness[J].Corrosion,1993,(10):850.doi:10.5006/1.3316009.
  • 6Yuan Pengbin,Guo Shengwu,Lv Shuanlu. Failure Analysis of High-Alloy Oil Well Tubing Coupling[J].Material Performance NACE International,2010,(08):68-71.
  • 7吕拴录,骆发前,陈飞,杨成新,李旭,聂采军,刘德英.牙哈7X-1井套管压力升高原因分析[J].钻采工艺,2008,31(1):129-132. 被引量:23
  • 8赵国仙,严密林,陈长风,路民旭,冯耀荣.影响碳钢CO_2腐蚀速率因素的研究[J].石油矿场机械,2001,30(B05):72-73. 被引量:25

共引文献3

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部