期刊文献+

孔型设计对棒材表面褶皱缺陷的影响及其优化 被引量:5

Influence of pass design on surface wrinkle defect of bar and its optimization
原文传递
导出
摘要 棒材表面褶皱缺陷是常见的产品缺陷之一,对河钢集团邯钢公司生产的棒材表面褶皱缺陷宏观形貌、金相组织进行了分析,结合轧钢生产,着重分析了孔型设计对产生褶皱缺陷的影响,并提出了粗轧孔型优化设计措施,有效地改善了棒材表面质量。 The surface wrinkle defect of bar is one of the common product defects,the macroscopic morphology and metallographic structure of wrinkle defects on the bar surface were analyzed,which produced by Hansteel Company of HBIS Group.Combined with rolling production,the influence of pass design on wrinkle defect was mainly analyzed,the optimization design measures of roughing rolling pass were put forward,which effectively improved the bar surface quality.
作者 刘斌 赵兴隆 李金波 许海平 刘永强 LIU Bin;ZHAO Xinglong;LI Jinbo;XU Haiping;LIU Yongqiang(Technology Center,Hansteel Company,HBIS Group,Handan 056015,China;Large Rolling Mill,Hansteel Company,HBIS Group,Handan 056015,China)
出处 《轧钢》 2021年第1期103-106,共4页 Steel Rolling
关键词 棒材 褶皱缺陷 孔型设计 优化 bar wrinkle defects pass design optimization
  • 相关文献

参考文献10

二级参考文献28

  • 1李慧峰.冷镦钢产品顶锻开裂的机理分析及应用[J].锻压技术,2006,31(2):1-4. 被引量:14
  • 2高志新,栾兆亮,李强,颜丙银.轧制缺陷对圆钢热顶锻性能的影响与辩识[J].轧钢,2007,24(1):69-72. 被引量:15
  • 3Colin Roy, Alfred R. Leger, et. Morgan's Compact Mill-Design Parameters, Application and Operational Benefits [ J ].Iron and Steel Engineer, 1982, (11): 149- 150.
  • 4Tadaaki yanazawa, Nobutsune Hiral, Teruaki Tanaka, et al.Development of grooveless rolling for a billet mill [J]. Iron and Steel Engineer, 1984, (8): 27- 32.
  • 5Weber R D.Wire rod rolling on flat rolls[J].WIREINDUSTRY,1975,(3):200-203.
  • 6李代钟.钢中的非金属平杂物[M].北京:科学出版社,1983
  • 7王延溥.轧钢工艺学[M].北京:冶金工业出版社,1981
  • 8北京钢铁学院.金属塑性变形与轧制原理[M].北京:北京钢铁学院出版社,1981
  • 9芦盛意.连铸坯质量[M].北京:冶金工业出版社,2004.
  • 10向亚云.钢铁冶炼技术工艺常见疑难问題解答及处理方法.广州:中国科技文化出版社.