摘要
通过试验制作出玄武岩与玻璃纤维复合水泥板,并以此为样品进行冻融试验、老化试验、耐碱性试验,模拟出真实的腐蚀环境,以测试经过处理后的样品水泥板。在相同的腐蚀环境中,碱性腐蚀对复合水泥板的影响作用最大,30 d内便可导致复合板黏结性能大幅度下降。
The composite cement board of basalt and glass fiber was made by experiment,and the freeze-thaw experiment,aging experiment and alkali resistance test were carried out as samples to simulate the real corrosion environment to test the treated sample cement board.In the same corrosion environment,alkaline corrosion has the greatest effect on the composite cement board,which can lead to a significant decrease in the bond properties of the composite board within 30 days.
作者
仝培周
TONG Peizhou(Northeastern University,Shenyang 110000,China)
出处
《混凝土》
CAS
北大核心
2021年第3期131-133,共3页
Concrete