摘要
以陶粒混凝土中的膨胀剂掺量(0、4%、8%、12%)和钢管壁厚(含钢率)为变量,制作了12组(24根)短柱,进行了轴压试验。结果表明:在本试验的膨胀剂掺量范围内,圆钢管微膨胀陶粒混凝土短柱试件的轴压承载力随膨胀剂掺量的增大而逐渐提高;根据试验结果建立了考虑膨胀剂掺量的受圆钢管约束微膨胀陶粒混凝土的强度准则计算公式,进而推导出了考虑膨胀剂掺量的圆钢管微膨胀陶粒混凝土短柱的极限承载力公式。
Taking the expansive agent content(0、4%、8%、12%)in ceramsite concrete and the steel tube(steel ratio)thickness as variables,12 groups of micro-expansive ceramsite concrete steel tubular(MECCST)short columns(24 specimens)were made,and the axial compression test was carried out.The results show that within the range of the expansion agent content in this experiment,the higher the expansion agent content,the higher the bearing capacity of the MECCST specimens.The formula for strength criterion of micro-expansive ceramsite concrete confined by steel tube which considering the expansive agent content is established by using the test datas,and the ultimate bearing capacity formula of MECCST short columns considering expansive agent content is deduced.
作者
李秀
朱红兵
韩帅
LI Xiu;ZHU Hong-bing;HAN Shuai(Wuhan Technical College of Communications,Wuhan 430065,China;College of Urban Construction,Wuhan University of Science and Technology,Wuhan 430065,China)
出处
《混凝土与水泥制品》
2021年第5期76-79,共4页
China Concrete and Cement Products
基金
国家自然科学基金资助项目(51778630)
湖北省教育厅科学研究计划项目(B2017559)。
关键词
钢管混凝土
微膨胀陶粒混凝土
短柱
轴压极限承载力
计算公式
Concrete filled steel tube short column
Micro-expansive ceramsite concrete
Short column
Ultimate axial compressive capacity
Calculation formula