摘要
针对某含钛难处理铀矿石,通过开展浸出剂浓度、浸出温度、氧化剂用量、氧分压、浸出时间、矿石粒度等条件试验,确定了适合该矿石的酸法加压浸出工艺路线。研究得到的浸出工艺路线,可有效降低浸出余酸和提高铀浸出率。
Research testing was carried out on a titanium-bearing uranium ore to solve the problems of poor leaching efficiency.The suitable pressure acid leaching process is determined based on the pressure acid leaching experimental study of leaching agent concentration,leaching temperature,oxygen fractional pressure,leaching time and ore granularity,etc.And the leaching process demonstrates many merits such as lowering residual acid,improving the uranium extraction and decreasing acid consumption.
作者
常喜信
钟平汝
李铁球
王高山
吴永永
CHANG Xixin;ZHONG Pingru;LI Tieqiu;WANG Gaoshan;WU Yongyong(Beijing Research Institute of Chemical Engineering and Metallurgy,CNNC,Beijing 101149,China)
出处
《铀矿冶》
CAS
2021年第2期123-127,共5页
Uranium Mining and Metallurgy
关键词
含钛铀矿
强化浸出
加压酸浸
搅拌浸出
titanium-bearing uranium ore
intensified leaching
pressure acid leaching
agitation leaching