摘要
对云南某地新开采硫、氧混合铅锌矿进行了浮选工艺实验研究。采用混合浮选硫化矿及氧化矿的工艺流程,获得了铅综合回收率85.18%、锌综合回收率95.46%的铅锌混合硫化精矿和氧化精矿,其中,硫化铅锌精矿中锌、铅品位分别为46.14%、7.86%;氧化铅锌精矿中铅、锌品位分别为12.71%、6.01%。浮选所得精矿满足冶金过程对原料的要求。研究成果可为浮选此类矿物提供参考依据。
An experimental study was carried out on flotation process of a newly mined mixed sulfide⁃oxide lead and zinc ore from Yunnan Province.By adopting a bulk flotation flow for the mixed sulfide⁃oxide ore,a mixed lead⁃zinc sulfide concentrate and a lead⁃zinc oxide concentrate were floated,with the total lead recovery of 85.18%and total zinc recovery of 95.46%.Among them,the lead⁃zinc sulfide concentrate graded 46.14%Zn and 7.86%Pb,while the lead⁃zinc oxide concentrate graded 12.71%Zn and 6.01%Pb.The flotation concentrates can meet the requirements of metallurgical process for raw materials.This research provides a reference for the succeeding flotation practice of such ores.
作者
毛志丹
谢克强
孔德全
苏开萌
袁晓磊
MAO Zhi-dan;XIE Ke-qiang;KONG De-quan;SU Kai-meng;YUAN Xiao-lei(Faculty of Metallurgical and Energy Engineering,Kunming University of Science and Technology,Kunming 650093,Yunnan,China;National Engineering Laboratory for Vacuum Metallurgy,Kunming 650093,Yunnan,China;Design and Research Institute,Kunming University of Science and Technology,Kunming 650051,Yunnan,China)
出处
《矿冶工程》
CAS
CSCD
北大核心
2021年第6期34-37,共4页
Mining and Metallurgical Engineering
基金
国家自然科学基金(51764033)。
关键词
铅锌矿
混合浮选
铅锌混合精矿
硫化铅锌精矿
氧化铅锌精矿
硫化剂
lead⁃zinc ore
bulk flotation
mixed lead⁃zinc concentrate
lead⁃zinc sulfide concentrate
lead⁃zinc oxide concentrate
sulfurizing agent