摘要
通过对Cr-Mo合金渗碳钢厚壁齿套锻坯进行不同加热温度和保温时间的等温正火工艺试验,最终确认该类齿套锻坯适宜的等温正火工艺参数为620℃×4 h。采用该等温正火工艺处理后,在锻坯的锻造连皮位置不会出现贝氏体或马氏体等异常组织,后续加工过程没有拉刀损坏现象。
Isothermal normalization process test is conducted with different heating temperature and heat preservation time for Cr-Mo alloy carburized steel thick-walled tooth sleeve forging blank,and the suitable isothermal normalization process parameters for this type of tooth sleeve forging blank is finally confirmed to be 620℃×4 h.After the isothermal normalization treatment,the forging blank will not have any abnormal structure such as bainite or martensite in the forging skin position,and there is no broach damage during the subsequent processing.
作者
陈郧
皇百红
张峰
杨亮波
张宇
孙睆睆
Chen Yun;Huang Baihong;Zhang Feng;Yang Liangbo;Zhang Yu;Sun Huanhuan(Material Technology Research Institute of Dongfeng Commercial Vehicle Technical Center,Shiyan 442001;Dongfeng Forging Co.,Ltd.,Shiyan 442012)
出处
《汽车工艺与材料》
2022年第3期20-23,共4页
Automobile Technology & Material
关键词
Cr-Mo合金渗碳钢
厚壁齿套锻坯
等温正火
工艺试验
Cr-Mo alloy carburized steel
Thick-walled tooth sleeve forging blank
Isothermal normalizing
Process test