期刊文献+

高硅型异极矿硫化—胺类捕收剂浮选机理研究 被引量:2

Study on Sulfide-amine Flotation Mechanism of Hemimorphite with High Content of Silicon
下载PDF
导出
摘要 采用浮选溶液化学理论结合第一性原理研究了高硅型异极矿硫化—胺类捕收剂浮选作用机理。研究表明,长链胺分子对异极矿回收率高于短链胺分子,直链胺分子的捕收能力优于同分子量的支链结构;矿浆pH值为11有利于异极矿与石英的分离,十八伯胺的适宜用量为1.25×10^(-4) mol/L;硫化钠可以显著提高异极矿回收率。溶液化学分析显示HS-是矿物表面活化作用的主要成分,且其浓度为(1.950~6.180)×10^(-3) mol/L时,矿物回收率均在85%以上。第一性原理计算表明HS-可以与异极矿表面Zn和O_(1)位点成键,但吸附作用不强;而十八伯胺与异极矿表面的吸附作用更弱,因此需要过量硫化才能有利于异极矿的浮选。 Sulfide-amine flotation mechanism of hemimorphite with high content of silicon was studied by solution chemistry theory and first principle calculation.Results show that the flotation recovery of hemimorphite by using long carbon chain amine is higher than that with short carbon chain amine,and the straight-chain amine is better than that of branched one.Satisfactory separation can be obtained when pulp pH is around 11,and the optimal dosage of octadecylamine is about 1.25×10^(-4) mol/L.Sodium sulfide can significantly increase the recovery of hemimorphite.Solution chemical analysis shows that the HS-is the active ingredient of hemimorphite surface activation,and the recovery of hemimorphite can reach greater than 85%when the concentration of HS-is from 1.950×10^(-3) mol/L to 6.180×10^(-3) mol/L.First principle calculation shows that HS-can weakly bond with the Zn and O_(1) atoms at hemimorphite surface,and the adsorption of octadecylamine at hemimorphite surface is weaker than that of HS-ions.
作者 许大洪 陈晔 XU Dahong;CHEN Ye(Guangxi Gaofeng Mining Co., Ltd., Nandan 547205, Guangxi, China;College of Resources, Environment and Materials, Guangxi University, Nanning 530004, Guangxi, China)
出处 《矿产保护与利用》 2022年第1期28-33,共6页 Conservation and Utilization of Mineral Resources
基金 国家自然科学基金(NSFC 51864003)。
关键词 异极矿 氧化锌矿 硫化 浮选 第一性原理 hemimorphite zinc oxide ore sulfide amine flotation first-principle calculation