摘要
Herein,we reported a method to prepare magnetic sodalite sphere by using the mud from backwash wastewater after polyaluminum chloride(PAC)coagulation.The results showed that approximately 100%of Fe in the wastewater was precipitated as flocculent iron mud(FM)by adding PAC.FM was converted to spherical magnetic sodalite(FMP)with a diameter of 3μm via a facile alkali hydrothermal method without adding Al/Si resources or reductant.The product FMP had the saturated magnetization of 10.9 emu g^(-1) and high Zn^(2+)adsorption capacity of 50.6 mg g^(-1).Without coagulation with PAC,the removal rate of Fe from the wastewater was only 92.7%,and the precipitated mud(RM)was converted to irregular particles(RMP),which had weak magnetic response and low capacity of Zn^(2+)adsorption comparing with FMP.With the method,the Fe in backwash wastewater was effectively recycled,and the generated sludge was converted to well-formed sodalite sphere without generating any secondary waste.
基金
This work was supported by the National Key Research and Development Program of China(Grant No.2019YFE0117900)
the National Natural Science Foundation of China(Grant Nos.52070038 and 51878134)
the Science and Technology Program of Jilin Province(Grant No.20190303001SF).