摘要 研究了不同质量分数的光整液残留对镀锌板表面三价铬钝化膜耐热性、耐溶剂性、耐指纹性、耐蚀性和涂装性能的影响。结果表明,光整液残留对三价铬钝化膜的耐热性、耐指纹性及耐溶剂性无明显影响。随着残留光整液质量分数增大,钝化膜耐蚀性逐渐变差;当残留光整液质量分数≥0.4%时,钝化膜的涂装性变差。 The effect of the mass fraction of finishing liquid which was left on zinc-coated steel on the properties of trivalent chromium passivation film i.e.its resistance to heat,solvent,fingerprint,and corrosion as well as coatability were studied.The results showed that the finishing liquid residue had no significant effect on the heat,fingerprint,and solvent resistance of trivalent chromium passivation film.With the increasing of the mass fraction of finishing liquid residue,the corrosion resistance of passivation film was decreased gradually.Its coatability became worse when the mass fraction of finishing liquid residue was 0.4%or higher.
作者 张百勇 王滕 杨平 柴立涛 李超 ZHANG Baiyong;WANG Teng;YANG Ping;CHAI Litao;LI Chao(Technology Center of Ma’anshan Iron and Steel Co.,Ltd.,Ma’anshan 243000,China)
出处 《电镀与涂饰》 CAS 北大核心 2022年第9期665-669,共5页 Electroplating & Finishing
基金 国家重点研发计划专项资助项目(2017YFB0304300,2017YFB0304305)。
关键词 光整液残留 三价铬钝化 耐蚀性 耐溶剂性 耐指纹性 涂装性 residue of finishing liquid trivalent chromium passivation corrosion resistance solvent resistance fingerprint resistance coatability
  • 相关文献

参考文献8

二级参考文献75

共引文献64

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部