摘要
河南某氧化钼矿石,钼品位为0.115%,氧化钼品位为0.081%,占总钼的70.43%。原矿破碎至-5 mm,用1%氢氧化钠溶液进行常温堆浸,采用破碎—堆浸—萃取—酸沉的工艺流程,获得钼酸铵产品。最终获得钼总浸出率60.83%,氧化钼浸出率90.12%,钼堆浸作业总回收率84.91%的技术指标。
A molybdenum oxide ore in Henan has a molybdenum grade of 0.115%and a molybdenum oxide grade of 0.081%,accounting for 70.43%of the total molybdenum.The raw ore is crushed to-5mm,and 1%sodium hydroxide solution is used for heap leaching at room temperature,and the ammonium molybdate product is obtained by the process of crushing-heap leaching-extraction-acid precipitation.Finally,the technical indicators of total molybdenum leaching rate of 60.83%,molybdenum oxide leaching rate of 90.12%and total recovery rate of molybdenum heap leaching operation of 84.91%are obtained.The leaching tailings can continue to use the flotation process for comprehensive recovery of molybdenum sulfide and lead minerals or for the manufacture of building materials.
作者
曹亮
刘燕
蒋丽娟
于晨
CAO Liang;LIU Yan;JIANG Li-juan;Yu Chen(Northwest Institute for Nonferrous Metal Research,Xi′an 710016,Shaanxi,China;College of Chemical Engineering and Environment,China University of Petroleum,Qingdao 266580,Shandong,China)
出处
《中国钼业》
2022年第3期42-45,共4页
China Molybdenum Industry
关键词
氧化钼矿石
粗粒级
堆浸
萃取
钼酸铵
molybdenum oxide ore
coarse grain size
heap leaching
extraction