为了了解不同消毒方式(紫外消毒、紫外-氯联合消毒、氯消毒)对管段出水水质及管段腐蚀的影响,在某水厂构建了一套管网系统中试装置进行研究。根据管垢形貌特征的变化发现,氯消毒方式下管垢的形成时间比紫外-氯消毒方式下要短;另外,管垢组分分析结果显示,在紫外消毒和紫外-氯联合消毒两种方式下,管垢各组分之间存在α-FeOOH/(γ-FeOOH+β-FeOOH+Fe_(3)O_(4))>1的关系,这表明紫外消毒和紫外-氯消毒两种方式可抑制管网腐蚀。
A pilot-scale device of pipe network system was constructed in a water treatment plant in order to investigate the influence of different disinfection methods(UV disinfection,UV/chlorine disinfection and chlorination)on the drinking water quality and pipe corrosion.According to the morphological characteristics of the pipe scale,the scale formation time of chlorination was shorter than that of UV/chlorine disinfection.In addition,the analysis of pipe scale components in both UV disinfection and UV/chlorine disinfection showed that the ratio ofα-FeOOH toγ-FeOOH+β-FeOOH+Fe_(3)O_(4) was greater than 1,indicating that the UV disinfection and UV/chlorine disinfection inhibited the corrosion of the pipe network.
作者
黄慧婷
邹放
王敏
顾军农
HUANG Hui-ting;ZOU Fang;WANG Min;GU Jun-nong(Beijing Engineering Research Center for Drinking Water Quality,Technology Institute of Beijing Waterworks Group Co.Ltd.,Beijing 100192,China)
出处
《中国给水排水》
CAS
CSCD
北大核心
2022年第13期42-45,共4页
China Water & Wastewater
基金
北京市科委项目(Z201100008220003)。
关键词
饮用水
紫外消毒
氯消毒
紫外-氯联合消毒
供水管网腐蚀
drinking water
UV disinfection
chlorination
UV/chlorine disinfection
corrosion of water supply pipe network