摘要
通过对漆膜形成过程的机理分析,揭示了漆层在干燥成膜过程中起泡形成的主要原因。通过采取严格控制漆层厚度、添加慢干稀释剂、延长底面漆喷涂时间间隔、提高操作技能等措施,有效解决了漆层起泡问题。
The main reason of blistering in the process of drying film was revealed by analyzing the mechanism of paint film formation.The blistering problem was effectively solved by strictly controlling the thickness of paint film,adding slow drying diluent,prolonging the time interval of bottom paint spraying and improving operation skills.
作者
钮京芳
NIU Jing-fang(Shijazhuang Haishan Industrial Development Co.,Ld.,Shijazhuang 050200,China)
出处
《现代涂料与涂装》
CAS
2022年第7期63-65,共3页
Modern Paint & Finishing
关键词
漆层起泡
表干时间
漆层厚度
时间间隔
blistering of paint film
surface drying time
paint film thickness
time interval