Load dependent microstructural evolution in an as-cast 26%Cr high chromium cast iron during unlubricated sliding

原文传递
导出
摘要 In the current study,an as-cast 26%Cr high chromium cast iron(HCCI)alloy was subjected to dry-sliding linear wear tests,under different loads.The loads were selected based on analytically computing the critical load(PC)i.e.,the load necessary to induce plastic deformation.The PC was calculated to be 15 N and accordingly,a sub-critical load(5 N)and an over-critical load(20 N)were chosen.The influence of increasing the load during the wear test was investigated in terms of the matrix microstructural behaviour and its ability to support the surrounding carbides.The morphological aspects of the wear tracks,and the deformed matrix microstructure adjacent and underneath the track was analysed by confocal laser scanning microscope(CLSM)and scanning electron microscope(SEM),respectively.No evidence of plastic deformation of the matrix was observed below PC.On the contrary,at loads equal to and higher than PC,the austenitic matrix plastically deformed as evidenced by the presence of slip bands.Electron backscattered diffraction(EBSD)measurements in terms of grain reference orientation deviation,and micro-Vickers hardness of the austenitic matrix indicated a deformation depth of about 40μm at the maximum applied load of 20 N.The active wear mechanisms during sliding were a combination of both adhesive and abrasive wear,although increasing the load shifted the dominant mechanism towards abrasion.This was primarily attributable to the increased propensity for carbide cracking and fracturing,combined with the inability of the hardened austenitic matrix surface and sub-surface to adequately support the broken carbide fragments.Moreover,the shift in the dominant wear mechanism was also reflected in the wear volume and subsequently,the wear rate.
出处 《Friction》 SCIE EI CAS CSCD 2022年第8期1258-1275,共18页 摩擦(英文版)
基金 The present work is supported by funding from the Deutsche Forschungsgemeinschaft(DFG,project:GU 2102/2-1).
  • 相关文献

参考文献2

二级参考文献23

  • 1Reich H.Optimized Crusher Selection for the Cement Industry[C]∥ThyssenKrupp Frdertechnik GmbH Processing.Magdeburg:[s.n.],2000:1.
  • 2Gundlach R,Janowak B J.Process Overview/Wear and Abrasion Testing[C]∥2nd International Conference on Austempered Ductile Iron:Your Means to Improved Performance, Productivity and Cost.New York:ASME,1986:23.
  • 3Yuri N P,Valentin G G,Hans B,et al.Surface Structure of Stainless and Hadfield Steel after Impact Wear[J].Wear, 2006,260(6):687.
  • 4Fucheng Z,Tingquan L.A Study of Friction-Induced Martensitic Transformation for Austenitic Manganese Steel [J]. Wear,1997,212(2):195.
  • 5Yan W,Fang L,Sun K,et al.Effect of Surface Work Hardening on Wear Behavior of Hadfield Steel[J].Materials Science and Engineering,2007,460-461A(6):542.
  • 6Dastur Y N,Leslie W C.Mechanism of Work Hardening in Hadfield Manganese Steel[J].Metallurgical and Materials Transactions,1981,12A(5):749.
  • 7Mosbah AY,Wexler D,Calka A.Abrasive Wear of WC-FeAl Composites[J].Wear,2005,258(9):1337.
  • 8Tianfu j,Fucheng Z.The Work-Hardening Behavior of Medium Manganese Steel Under Impact Abrasive Wear Condition [J].Materials Letters,1997,31(5):275.
  • 9Zhang G S,Xing J D,Gao Y M.Impact Wear Resistance of WC/Hadfield Steel Composite and its Interfacial Characteristics [J].Wear,2006,260(7-8):728.
  • 10Li D,Liu L,Zhang Y,et al.Phase Diagram Calculation of High Chromium Cast Irons and Influence of Its Chemical Composition[J].Materials and Design,2009,30(2):340.

共引文献14

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部