摘要 采用层叠烧结法制备多孔TC4钛合金,并对其显微结构进行表征。通过对比多孔和实体钛合金表面的成骨细胞黏附和铺展情况以及细胞毒性测试结果,研究了多孔钛合金表面的生物活性并探讨了其作用机制。结果表明:层叠烧结多孔钛合金呈现规则的网孔结构,孔隙尺寸在一百到几百微米之间,满足骨长入要求。多孔钛合金无毒,较实体钛合金具有更好的生物相容性。 Porous TC4 titanium alloy was prepared by a stacked-forced-sintering method,and its microstructure was characterized.By comparing the adhesion and spread of osteoblasts on the surface of porous and solid titanium alloy and the results of cytotoxicity test,the biological activity on the surface of porous titanium alloy and its mechanism were studied.The results showed that the stacked-forced-sintered porous titanium alloy exhibited regular mesh structure,and the pore size was between one hundred and several hundreds of microns,which met the requirements of bone ingrowth.Porous titanium alloy is non-toxic and has better biocompatibility than solid titanium alloy.
作者 张云龙 李若琳 ZHANG Yunlong;LI Ruolin(School of Materials Engineering,Jiangsu University of Technology,Changzhou Jiangsu 213001,China)
出处 《上海金属》 CAS 2023年第1期20-25,共6页 Shanghai Metals
关键词 烧结 多孔 钛合金 生物相容性 sintering porous titanium alloy biocompatibility
  • 相关文献

参考文献6

二级参考文献62

  • 1王勃生,孙福玉,孟庆恩,高振英.第三代生物医学材料的研究与开发[J].材料科学与工程,1994,12(1):1-4. 被引量:8
  • 2史胜凤,林军,周炳,王小祥.医用钴基合金的组织结构及耐腐蚀性能[J].稀有金属材料与工程,2007,36(1):37-41. 被引量:12
  • 3MACDONALD D E,RAPUANO B E,DEO N,STRANICK M,SOMASUNDARAN P,BOSKEY A L.Thermal and chemical modification of titanium-alumium-vanadium implant materials effects on surface properties,glycoprotein adsorption,and MG63 cell attachment[J].Biomaterials,2004,25(16):3135-3146.
  • 4GARRETT R,ABHAY P,DIMITRIOS P A.Fabrication methods of porous metals for use in orthopaedic applications[J].Biomaterials,2006,27(13):2651-2670.
  • 5HOLY C E,FIALKOV J A,DAVIES J E,SHOICHET M S.Use of a biomimetic strategy to engineer bone[J].J Biomed Mater Res A,2003,65(4):447-453.
  • 6ITALA A I,YLANEN H O,EKHOLM C,KARLSSON K H,ARO H T.Pore diameter of more than 100 micron is not requisite for bone ingrowth in rabbits[J].J Biomed Mater Res,2001,58(6):679-683.
  • 7MAITZ M F,POON R W,LIU X Y,PHAM M T,CHU P K.Bioactivity of titanium following sodium plasma immersion implantation and deposition[J].Biomaterials,2005,26(27):5465-5473.
  • 8KOKUBO T,KUSHITANI H,SAKKA S,KITSUGI T,YAMAMURO T.Solutions able to reproduce in vivo surface-structure changes in bioactive glass-ceramics A-W3[J].Journal of Biomedical Materials Research,1990,24(6):721-734.
  • 9ST-PIERRE J P,GAUTHIER M,LEFEBVRE L P,TABRIZIAN M.Three-dimensional growth of differentiating MC3T3-E1 pre-osteoblasts on porous titanium scaffolds[J].Biomaterials,2005,26(35):7319-7328.
  • 10SERGO V,SBAIZERO O,DAVID R C.Mechnical and chemical consequences of the residual stresses in plasma sprayed hydroxyaptite coatings[J].Biomaterials,1997,18(6):477-484.

共引文献58

同被引文献12

引证文献1

二级引证文献2

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部