本研究以壳聚糖(CS)和马来酸酐(MA)为主要原料,通过TEMPO氧化法制备马来酰化壳聚糖(MAAC),并将其作为添加剂用于透析纸的制备。探究了CS和MA质量比对MAAC取代度及溶解度的影响,以及MAAC用量对透析纸物理性能、透气性和抗菌性的影响。结果表明,当m(CS)∶m(MA)∶m(TEMPO)=1∶1.0∶0.08时,MAAC的取代度较高且溶解性较好;在中性和碱性条件下,溶液透光率大于80%。当MAAC用量为2.0%时,透析纸的干、湿抗张指数和撕裂指数分别提高了10.0%、96.8%和20.3%,透气度达8.98μm/(Pa·s),并具有良好的抗菌性。
In this study, chitosan(CS) and maleic anhydride(MA) were used as the main raw materials to prepare maleoyl chitosan(MAAC)via TEMPO oxidation. The dialysis paper was prepared with the MAAC as the additives. The effects of the mass ratio of CS and MA on the substitution degree and solubility of the MAAC were studied, and the effects of MAAC dosage on the physical properties, air permeability and antibacterial properties of dialysis paper were also investigated. The results showed that the substitution degree of MAAC was higher and the solubility was better when the mass ratio of CS, MA and TEMPO was 1∶1. 0∶0. 08, and the light transmittance of the solution was greater than 80% under neutral and alkaline conditions. The dry and wet tensile index and tear index of dialysis paper after adding 2. 0%MAAC were increased by 10. 0%, 96. 8% and 20. 3%, respectively. The air permeability of dialysis paper after adding 2. 0% MAAC reached 8. 98 μm/(Pa·s), with a good antibacterial property.
作者
左金华
章飞洋
吴锦涵
王慧乐
伊财富
赵会芳
沙力争
ZUO Jinhua;ZHANG Feiyang;WU Jinhan;WANG Huile;YI Caifu;ZHAO Huifang;SHA Lizheng(School of Environmental and Natural Resource,Zhejiang University of Science and Technology,Hangzhou,Zhejiang Province,310023;Zhejiang Hengda New Material Co.,Ltd.,Quzhou,Zhejiang Province,324401)
出处
《中国造纸》
CAS
北大核心
2023年第1期9-16,共8页
China Pulp & Paper
基金
浙江省重点研发计划(2021C01094)
衢州市科技计划项目(2021K48)。
关键词
壳聚糖
马来酸酐
透析纸
物理性能
抗菌性
chitosan
maleic anhydride
dialysis paper
physical properties
antibacterial property