摘要
四川某铁矿石主要有用矿物为磁铁矿。随着矿石向深部开采,现有工艺流程已不适于其深部矿石,在对深部矿石进行选矿工艺实验研究时,引入细筛工艺,大大降低了第二段磨矿的细度,降低其能耗。研究结果表明,采用干式磁选预选-二段磨矿二段磁选-磁选精矿细筛的选矿工艺流程,可获得全铁品位60.24%、全铁回收率88.67%的铁精矿。
The main useful mineral of the iron ore in Sichuan is magnetite.With deep mining of ore, the existing technological process is not suitable for the deep ore.The fineness of the second stage grinding is greatly reduced by adding the fine screen technology in the experimental study of the deep ore dressing process.The results show that the iron concentrate with the total iron grade of 60.24% and the total iron recovery of 88.67% can be obtained by adopting the beneficiation process of dry magnetic preseparation and discarding-two stage grinding, two stage magnetic separation and one fine screen of magnetic concentrate.
作者
陈宏凯
杜新
王艳
Chen Hongkai;Du Xin;Wang Yan(Sichuan Jin Ning Mining Co.,Ltd.,Liangshan,Sichuan,China;Sichuan Xiye Testing Technology Co.,Ltd.,Chengdu,Sichuan,China)
出处
《矿产综合利用》
CAS
北大核心
2023年第1期168-171,共4页
Multipurpose Utilization of Mineral Resources
关键词
磁铁矿
深部矿石
预选抛尾
细筛
磨矿
Magnetite
Deep ore
Preseparation and discarding
Fine screen
Ore grinding