摘要
Six novel hydrolytically degradable polyesters were synthesized from thiodipropionic acid(TDPA)and five diols by melt polycondensation,and characterized by FT-IR,1H NMR,gel permeation chromatography,differential scanning calorimetry and thermogravimetry analysis.The polystyrene-equivalent number-average(Mn)and weight-average molecular weight(Mw)of these polyesters ranged from 4900-11100 Da and 7900-20879 Da,respectively,with PDI values of 1.48-1.98.The melting point varied from 62.3-127.9℃,and the 50%mass-loss temperature ranged between 387-417℃.The degradation of these polyesters was studied in terms of relative weight loss in distilled water at different pH.Weight losses of 14%-26%were obtained at pH 7.0,26%-38%at pH 6.0,and 32%-43%at pH 8.3 over a 20-week period.The ecotoxicity study suggested that safety of the synthesized polyesters for the eisenia foetida.These results indicate that these polyesters have a combination of good thermal and degradability behaviors,which can be tailored through selection of the diol monomers used in the synthesis.
基金
Funded by the Program (BG20190227001)of High-end Foreign Experts of the State Administration of Foreign Experts Affairs (SAFEA)
the Coal Conversion and New Carbon Materials Hubei Key Laboratory at Wuhan University of Science and Technology (WKDM202005)。