Effects of MgO/Al_(2)O_(3)and CaO/SiO_(2)ratios on viscosity of high titaniumbearing blast furnace slag

原文传递
导出
摘要 The effects of MgO/Al_(2)O_(3)and CaO/SiO_(2)ratios on the viscosity,break-point temperature,and viscous activation energy of a high titanium-bearing slag were studied.The results showed that both the viscosity and the break-point temperature of the slag decreased with the MgO/Al_(2)O_(3)ratio increasing from 0.50 to 0.65,the viscous activation energy decreased gradually,and the thermal stability became better.In addition,with an increase in CaO/SiO_(2)ratio from 1.12 to 1.22,the main viscous units in the slag depolymerized and the viscosity of slag decreased.However,the break-point temperature of slag showed an increasing tendency.The viscous activation energy decreased gradually and the thermal stability became better.The basic phase in the experimental high titanium-bearing slag was pyroxene,and its amount increased with increasing the MgO/Al_(2)O_(3)ratio while decreased with increasing the CaO/SiO_(2)ratio.
出处 《Journal of Iron and Steel Research(International)》 SCIE EI CAS CSCD 2023年第3期456-464,共9页 钢铁研究学报(英文版)
基金 The authors were specially grateful to the National Natural Science Foundation of China(Grant No.51904063) the Fundamental Research Funds for the Central Universities(N2025023).
  • 相关文献

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部