某硫化铜矿含Cu约0.8%,采用X射线分选技术预选粗碎后≥30 mm的铜矿石,抛废率27%,抛出废石含Cu 0.09%,预选作业回收率96.95%。预选后入选品位提高0.2个百分点、选比由29.85 t/t降至22.68 t/t。年采出规模30万t铜矿,粗碎后≥30 mm预选,年创效339.7万元。
A copper sulfide ore contains about 0.8%Cu.The X-ray separation technology is used to preconcentrate copper ore that is more than 30 mm after coarse crushing.The scrap rate is 27%and the scrap Cu is 0.09%,and the recovery is 96.95%.After preselection,the selected grade increased by 0.2 percentage points,and the selection ratio decreased from 29.85/t to 22.68 t/t.The annual production scale of 300000 t copper ore,coarse crushed≥30 mm preselected,annual efficiency of 3.397 million yuan.
作者
王彩虹
魏有林
张丽丽
WANG Caihong;WEI Youlin;ZHANG Lili(Gansu Jiu Steel Group Hongxing Iron&Steel Co.Ltd.,Jiayuguan 735100,China)
出处
《甘肃冶金》
2023年第4期1-4,共4页
Gansu Metallurgy
关键词
铜矿
X射线
预选
浮选
选比
copper ore
X-ray
preconcentration
flotation
ratio