摘要
通过对苏里格气田东区站场排液弯管的腐蚀形貌观察、腐蚀产物检测和现场挂片试验,明确了弯管的腐蚀形式为冲刷腐蚀。利用多相流模拟软件对弯管处介质的分布特点、壁面剪切应力和冲蚀速率进行模拟,模拟结果表明:冲刷腐蚀的主要影响因素为介质流速和固相颗粒含量;弯管内弧主要受液相高流速产生的壁面剪切应力影响,外弧主要受固相颗粒的冲击磨损作用影响。根据苏里格东区站场排液弯管的腐蚀风险特点,推荐在高风险位置使用玻璃钢管或者陶瓷内衬弯管进行腐蚀防治。
It was determined that the corrosion form of the drainage elbow in the East station of Sulige gas field was erosion corrosion,according to the corrosion morphology observation,corrosion product detection and field coupon test.Multiphase flow simulation software was used to simulate the distribution characteristics of the medium,wall shear stress and erosion corrosion rate.The simulation results showed that the main influencing factors of erosion corrosion were medium velocity and solid particle content.The inner arc of the elbow was mainly affected by wall shear stress caused by high liquid flow rate,and the outer arc of the elbow was mainly affected by impact wear of solid particles.According to the corrosion risk characteristics of the drainage elbow in the East station of Sulige gas field,it was recommended to use glass fiber reinforced plastic pipe or ceramic lined elbow in high risk locations for corrosion prevention.
作者
常鹏
李先兵
李凯
韩炜
温宁华
王毛毛
CHANG Peng;LI Xianbing;LI Kai;HAN Wei;WEN Ninghua;WANG Maomao(The No.5 Gas Production Plant,Changqing Oil-Field Company,Wushenqi 017300,China;Safetech Research Institute,Beijing 102209,China)
出处
《腐蚀与防护》
CAS
CSCD
北大核心
2023年第8期46-50,82,共6页
Corrosion & Protection
关键词
排液管线
腐蚀风险
冲刷腐蚀
壁面剪切应力
固相颗粒
drainage pipeline
corrosion risk
erosion corrosion
wall shear stress
solid particle