摘要
针对太钢峨口铁矿资源及生产现状,开展了二段磁选精矿提铁降杂试验研究,采用磨矿-弱磁选-反浮选流程,可获得产率76.33%、TFe品位69.93%、回收率93.08%、SiO_(2)含量1.63%的高品质铁精矿。
In view of the resource characteristics and production status of Ekou Iron Mine of Taiyuan Iron&Steel(Group)Co Ltd,an experimental research was conducted to upgrade iron grade of the concentrate from the second-stage magnetic separation while reducing impurities therein.An optimized flowsheet consisting sequentially of grinding,low-intensity magnetic separation and reverse flotation was adopted in the experiment,resulting in a high-quality iron concentrate grading 69.93%TFe at a recovery of 93.08%,with a yield of 76.33%,while the SiO_(2) content was reduced to 1.63%.
作者
米子军
罗良飞
李宗蔚
钟志刚
MI Zijun;LUO Liangfei;LI Zongwei;ZHONG Zhigang(Mining Branch of Taiyuan Iron&Steel(Group)Co Ltd,Taiyuan 030027,Shanxi,China;Changsha Research Institute of Mining and Metallurgy Co Ltd,Changsha 410012,Hunan,China)
出处
《矿冶工程》
CAS
北大核心
2023年第6期88-91,共4页
Mining and Metallurgical Engineering
关键词
铁精矿
脱硅
提铁降杂
磨矿
磁选
反浮选
iron concentrate
desilication
upgrading iron grade whilst reducing impurities
grinding
magnetic separation
reverse flotation