摘要
为验证湖南某白钨矿分级-重选联合预抛废在工业上的可行性,进行了工业分流试验和浮选对比小型试验。结果表明,在适宜条件下,采用筛分-螺旋溜槽预抛工艺,可抛掉产率25.50%、钨品位0.034%、钨损失率2.99%的抛废产品;抛废后再进行浮选,精矿产品品位和回收率均高于分级溢流直接浮选所得精矿产品。
To examine the industrial feasibility of pre⁃discarding by using screening classification combined with gravity separation in processing of a scheelite ore from Hunan Province,industrial distributary and flotation trial tests were carried out.The results show that a process consisting of screening and spiral chute discarding under optimized conditions can discard tailings grading 0.034%WO3 with a yield of 25.50%in mass,leading to tungsten loss of only 2.99%.With this pre⁃discarding before flotation process,both the grade and recovery of the final flotation concentrate are improved,compared to the concentrate obtained from direct flotation of overflow product.
作者
石志中
罗云波
何军
张发明
刘国清
韩雷
SHI Zhizhong;LUO Yunbo;HE Jun;ZHANG Faming;LIU Guoqing;HAN Lei(Hunan Nonferrous Xintianling Tungsten Industry Co Ltd,Chenzhou 423000,Hunan,China;Guangzhou Yueyouyan Mineral Resources Technology Co Ltd,Guangzhou 510651,Guangdong,China)
出处
《矿冶工程》
CAS
北大核心
2024年第2期66-70,共5页
Mining and Metallurgical Engineering
关键词
白钨矿
分级
重选
预抛废
筛分
螺旋溜槽
工业分流
浮选
钨
scheelite
classification
gravity separation
pre⁃discarding
screening
spiral chute
industrial distributary
flotation
tungsten