摘要
热轧圆钢产品对直线度要求高,直线度差会增加客户切损率。长钢轧钢厂针对连续发生的多起高棒圆钢因直线度差的质量异议,找出导致直线度差的原因,通过改造转毂、矫直冷床齿条以及降低精整工序钢材温度,有效提高了高棒圆钢产品质量。
Hot rolled round steel products have high straightness requirements,and the straightness difference will increase the cutting rate of customers.As to the quality objections occurred in Changgang high-bar round steel due to the straightness difference,the high-bar effectively improves the straightness of high-bar round steel products and reduces the quality problems by the transformation of the boss,the straightening of the cold bed rack,and the reduction of the finishing process steel temperature.
作者
李罗扣
詹卫金
第五文博
宫叶茂
Li Luokou;Zhan Weijin;Di Wuwenbo;Gong Yemao(Steel Rolling Plant of Shougang Changzhi Iron and Steel Co.,Ltd.,Changzhi Shanxi 046000,China)
出处
《山西冶金》
CAS
2024年第4期152-153,156,共3页
Shanxi Metallurgy
关键词
圆钢
直线度
转毂改造
冷床齿条
剪切温度
round steel
straightness
hub transformation
cold bed rack
shear temperature