摘要
镍钼矿选矿是有价元素提取的关键过程,会为后续矿产资源开发奠定基础。本案例中的镍钼矿中镍含量为0.52%、钼含量0.74%,呈现出集合产出形态。为实现对矿产资源的良好开发,按照工艺流程脱质后,将CMC作为抑制剂,使用浮选工艺处理,选矿实验得到的镍、钼回收率,分别为81.22%、72.55%,有利于降低后续矿产焙烧投入的成本,提高镍钼矿冶炼效率。
Nickel molybdenum ore beneficiation is a key process for extracting valuable elements,which will lay the foundation for subsequent mineral resource development.In this case,the nickel molybdenum ore has a nickel content of 0.52%and a molybdenum content of 0.74%,showing a collective production pattern.In order to achieve good development of mineral resources,CMC was used as a depressant after the process flow was carried out,and flotation technology was used for treatment.The recovery rates of nickel and molybdenum obtained from beneficiation experiments were 81.22%and 72.55%,respectively.This is beneficial for reducing the cost of subsequent mineral roasting investment and improving the smelting efficiency of nickel molybdenum ore.
作者
刘彬
LIU Bin(China Steel Group Shandong Mining Co.,Ltd,Linyi 276000,China)
出处
《世界有色金属》
2024年第8期126-128,共3页
World Nonferrous Metals
关键词
镍钼矿
选矿方案
磨矿细度
浮选条件
nickel molybdenum ore
Mineral processing plan
Grinding fineness
Flotation conditions