摘要
以共沉淀为基础,主要研究了反应制备过程镍钴锰硫酸盐溶液、碱液、氨液的进料顺序和进料位置、进料管个数和进料温度对制备产品Ni_(0.55)Co_(0.5)Mn_(0.40)(OH)_(2)的影响。结果表明采用采用镍钴锰硫酸液、氨液、碱液的进料顺序;镍钴锰硫酸液上进料,碱氨液下进料;镍钴锰硫酸液和碱液两点进料、氨一点进料;镍钴锰硫酸液进料温度40~45℃可以合成较高性能的Ni_(0.55)Co_(0.5)Mn_(0.40)(OH)_(2)产品。
Based on coprecipitation,in this paper,the effects of feeding sequence,feeding position,feeding tube number and feeding temperature of nickel-cobalt-manganese sulfate solution,alkali solution and ammonia solution on Ni_(0.55)Co_(0.5)Mn_(0.40)(OH)_(2) were studied.The results show that Ni_(0.55)Co_(0.5)Mn_(0.40)(OH)_(2) with high performance can be synthesized through method that Ni-Co-Mn liquid,ammonia liquid and alkali liquid as feeding sequence,Ni-CoMn liquid is fed up,alkali-ammonia liquid is fed down,Ni-Co-Mn liquid and alkali liquid are fed two points and 40-45℃ feeding temperature of Ni-Co-Mn solution.
作者
刘纪迎
李志林
刘飞
李鹏
杨永生
LIU Jiying;LI Zhilin;LIU Fei;LI Peng;YANG Yongsheng(Ningxia Zhongse New Material Co.,Ltd.,Shizuishan 753000,China)
出处
《粉末冶金工业》
CAS
北大核心
2024年第3期75-78,84,共5页
Powder Metallurgy Industry