摘要
针对某1250 mm热连轧生产线在精轧机轧制时经常出现带钢跑偏轧破、轧废的现象,从温度控制、粗轧板形控制、轧辊不均匀磨损、轧辊冷却水、轧制润滑、轧机间隙、设备对中等方面进行逐一排查整改,最终将跑偏降级轧废控制在合理范围内。
In this paper,a 1250 mm hot continuous rolling production line in the finishing mill often occurred strip deviation rolling broken,The phenomenon of rolling waste is checked and rectified one by one from the aspects of temperature control,rough rolling shape control,roll uneven wear,roll cooling water,rolling lubrication,rolling mill gap and equipment,and finally the running deviation and demotion rolling waste is controlled within a reasonable range.
作者
李爱彬
杨少东
宋华东
Li Aibin;Yang Shaodong;Song Huadong(Guangxi Shenglong Metallurgical Co.,Ltd,Fangchenggang,538000,China)
出处
《冶金信息导刊》
2024年第4期48-50,共3页
Metallurgical Information Review
关键词
热轧带钢
跑偏
对中
润滑
间隙
hot strip
misalignment
lubrication
clearance