摘要 实木复合地板是市面上广泛应用的装饰材料之一,静曲强度和弹性模量是判定其质量好坏的重要参数,而含水率则是影响其静曲强度和弹性模量的重要因素之一。文章通过对同一实木复合地板在不同含水率条件下的静曲强度与弹性模量进行测试,得出静曲强度与弹性模量均随含水率升高而先增大后减小,并均在含水率为9%左右取得最大值的结论,为生产制造、检验检测、实际应用以及标准的修订提供参考。 Solid wood composite flooring is one of widely used decorative materials in the market.Static bending strength and elastic modulus are important parameters to judge its quality,and water content is one of the important factors affecting its static bending strength and elastic modulus.In this paper,the static bending strength and elastic modulus of the same solid wood composite floor under different water content conditions are tested,and it is concluded that the static bending strength and elastic modulus increase first and then decrease with the increase of water content.The maximum value is reached at about 9%,which provides references for manufacturing,inspection and testing,practical application,and revision of standards.
作者 杨凇 欧阳启东 钱嘉伟 彭欢 时常杰 YANG Song;OUYANG Qidong;QIAN Jiawei;PENG Huan;SHI Changjie(Jiangsu Construction Engineering Quality Testing Center Co.,Ltd,Nanjing Jiangsu 210046 China)
出处 《江苏建筑》 2024年第4期137-139,共3页 Jiangsu Construction
关键词 实木复合地板 含水率 静曲强度 弹性模量 solid wood composite flooring moisture content static bending strength elastic modulus
  • 相关文献

参考文献7

二级参考文献36

  • 1龙玲,陆熙娴,井上明生.干燥器法测定木制品甲醛释放量的研究[J].林业科学,2004,40(4):148-152. 被引量:13
  • 2池永亮.浸渍纸主要性能指标对强化木地板压贴质量的影响[J].人造板通讯,2005,12(7):20-23. 被引量:4
  • 3王凤鸣.中密度纤维板断面密度分布的控制[J].林产工业,1996,23(4):27-32. 被引量:15
  • 4吴智慧.复合地板的生产工艺技术[J].林产工业,1997,24(2):41-43. 被引量:14
  • 5GB18580-2001.室内装饰装修材料—造板及其制品中甲醛释放限量[S].[S].,..
  • 6ROFFAEL E. Formaldehyde release from particleboard and other wood based panels[M]. Berlin: Forest Research Institute Malaysia,1993:29-134.
  • 7MYERS G E. Formaldehyde emission from particleboard and plywood paneling: measurement, mechanism, and product standards[J]. Forest Prod J, 1983, 33(5): 27-37,.
  • 8MEYER B, KOSHLAP K, GEISLING K L, et al. Comparison of wet and dry desiccator test methods for formaldehyde emission from UF-bonded wood products[J]. Forest Prod J, 1983, 33(1): 35-37.
  • 9RYBICKY J, HORST K, KAMBANIS S M. Assessment of the 2-hour desiccator test for formaldehyde release from particleboard[J]. Forest Prod J, 1983, 33(9): 50-54.
  • 10ROFFAEL E, MENZEL W. Influence of marginal condition on the determination of extractable formaldehyde by the perforator method[J]. Holz als Roh-Werkstoff, 1980, 38: 85-88.

共引文献23

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部