利用石材加工厂的石粉、石渣等废弃物为原料 ,应用优选法试验获得地面花砖基层用料 (不含水量 )配方 ,其质量比为水泥∶石粉∶碎石 =1∶2 .4∶2 .6.用该配方生产的地面花砖经物理力学性能测试 ,其抗折指标符合国家标准 .
Using stone powders and residues from stone processing factory as raw materials,applying the optimization to experiment in the fundamental layer of floor brick,a new formula is obtained.The mass ratio of cement,stone powder and broken stone is 1 ∶2.4∶ 2.6 ,through mechanical test the anti break index of the floor brick satisfies the national standard.