摘要
It was demonstrated that some level of order exists in glassy poly(ethylene terephthalate) by depolarized light intensity(DLI) technique, but this order is different from that in crystalline PET. The degree of order in glassy PET decrease with increasing temperature between 288-343 K. The active energy of this transition is about 22 56 kJ/mol. The IR analysis indicated that this order relates to gauche structure of the ethyleneglycol fragments. The decrease of order with temperature comes from the increase of distance between the order segments.
It was demonstrated that some level of order exists in glassy poly(ethylene terephthalate) by depolarized light intensity(DLI) technique, but this order is different from that in crystalline PET. The degree of order in glassy PET decrease with increasing temperature between 288-343 K. The active energy of this transition is about 22 56 kJ/mol. The IR analysis indicated that this order relates to gauche structure of the ethyleneglycol fragments. The decrease of order with temperature comes from the increase of distance between the order segments.
出处
《高等学校化学学报》
SCIE
EI
CAS
CSCD
北大核心
2003年第2期362-364,共3页
Chemical Journal of Chinese Universities