表面处理对亲水铝箔持续亲水性的影响 被引量:9

Influence of Surface Treatment on the Protracted Hydrphilicity of Hydrophilic Aluminium Foil
下载PDF
导出
摘要 通过测定水洗200h后,水滴在亲水铝箔表面接触角的方法来确定脱脂和铬化对亲水铝箔持续亲水性的影响。发现只要清洗彻底,则持续亲水性与脱脂剂的种类无关。铬化对持续亲水性的影响很大,用磷酸铬酸盐法处理的铝箔,其持续亲水性比用铬酸盐法处理的要好。用磷酸铬酸盐法于30℃,将铝箔处理3min,最后涂布亲水涂层得到的亲水铝箔,其持续亲水性最佳,水冲200h后,接触角为9~11°。 By testing the contact angle of water drop on the surface of the hydrophilic aluminium foil which has been deposited in flowing water for 200 hours, the influences of degreasing and chromate treating process on its protracted hydrophilicity are described . It is found that the protracted hydrophilicity is independent on the sort of the degreaser if it can remove oil and soil from the aluminium's surface completely and the chromate treating process influence the protracted hydrophilicity greatly.With respect to protracted hydrophilicity,the aluminium which is treated by the chromate-phosphate process is better than that by the chromate process. When the former is used to treat the alumininm foil, the optimum temperature is 30℃ and the optimum time is 3min.
出处 《表面技术》 EI CAS CSCD 北大核心 2003年第1期51-54,共4页 Surface Technology
关键词 脱脂 铬化 持续亲水性 接触角 Degreasing Chromate treating process Protracted hydrophilicity Contact angle
  • 相关文献

参考文献1

二级参考文献6

  • 1戴至成,硅化合物的生产与应用,1994年,170页
  • 2张策,涂料工业,1993年,1卷,15页
  • 3吴纯素,化学转化膜,1988年,72页
  • 4王致禄,聚合物胶粘剂,1985年,82页
  • 5匿名著者,国际标准ISO1462-1973(E)
  • 6匿名著者,中国国家标准GB6458-86

共引文献12

同被引文献49

引证文献9

二级引证文献21

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部