用Larson-Miller参数描述12Cr1 MoV与15CrMo的老化行为 被引量:12

Aging behavior descriptions for main steam pipe steels 12Cr1MoV and 15CrMo byLarson-Miller parameter
下载PDF
导出
摘要 通过系列温度-时间组合的实验室模拟实验和对大量数据的汇总、分析,证明Larson-Miller(P)参数可以合理描述12Cr1MoV、15CrMo等主蒸汽管道材料的多种老化行为.结果表明,随着P值的增大,热管材料基体中的合金元素贫化加剧,球化程度逐渐升高,且力学性能显著下降,显示出这两种主蒸汽管道材料的组织和力学性能退化与Larson-Miller参数之间良好的对应关系. By means of series of comprehensible temperature-time simulating experiments and collection and analysis of a great deal of the published data, it is proved that Larson-Miller(P) parameter can rationally describe aging behaviors of main steam pipe steels, such as 12Cr1MoV and 15CrMo. It is concluded that with the increasing of P parameter, the dilution of alloy elements in matrix quickens, extent of spheroidizing gradually enhances and mechanical properties degenerate. It can be seen obviously that the degradation analysis of both the microstructure and mechanical properties for these two main steam pipe steels shows a good relationship with Larson-Miller parameter.
出处 《材料科学与工艺》 EI CAS CSCD 2002年第4期395-398,共4页 Materials Science and Technology
基金 甘肃省自然科学基金资助项目(ZS001-A22-046-C)
关键词 12CrlMoV 15CrMo 老化 Larson-Miller参数 珠光体耐热钢 主蒸汽管道 材料 电厂 锅炉 aging Larson-Miller parameter pearlitic resistant steel main steam pipe material
  • 相关文献

参考文献7

二级参考文献16

  • 1周顺深.炉管珠光体球化与破裂寿命的关系[J].华东电力,1995,23(5):7-11. 被引量:10
  • 2钟土红.钢的回火工艺和回火方程[M].北京:机械工业出版社,1993..
  • 3郭宏.北京科技大学博士学位论文[M].,1995..
  • 4陈国良 郭宏 等.-[J].北京科技大学学报,1997,19:157-157.
  • 5贝茵EC.钢中的合金元素[M].北京:中国工业出版社,1996.193.
  • 6方嘉礼,机电工程金属材料手册,1997年,3页
  • 7符长璞,金属热处理,1992年,3期,21页
  • 8李兵,电力技术,1982年,1期,2页
  • 9吴非文,高温金属运行,1978年
  • 10邢鼎年,电厂用耐热钢,1976年

共引文献47

同被引文献79

引证文献12

二级引证文献86

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部