摘要
介绍了4种层状锰氧化物的合成方法,即水热法,离子交换法,溶胶—凝胶法,高温固相法。水热法及离子交换法的反应温度低,反应条件温和且水热法可以一步得到产物;高温固相法简单易行;溶胶—凝胶法所制得产物的颗粒细小,均匀。
The present paper introduces 4 ways of composing layered manganese oxide, i.e. hydrothermal, ionic exchange, solgel and high temperature solidoid. The hydrothermal and ionic exchange can achieve both a low reaction temperature and a temperate reaction condition. Moreover, the hydrothermal can bring out the composites at one step. The high temperature solidoid is easy to perform, while the sol-gel can produce tiny and uniform granules.
出处
《中国锰业》
2003年第1期4-6,共3页
China Manganese Industry
基金
广东省自然科学基金(011443)