摘要
通过下冷铁等工艺措施,采用1.5t·h冲天炉成功地生产出7.5t铸件,并详细介绍了该铸件的造型及浇注工艺。
By using inner densener and other process measures,a7.5t heavy casting was successfully produced with a1.5t·h -1 cupola.The foundry method and pouring process for the casting was intro-duced in detail.
出处
《现代铸铁》
CAS
2003年第1期32-33,共2页
Modern Cast Iron