摘要
介绍了PAC捕收剂代替OSN - 43 # 捕收剂用于凤凰山铜矿选矿厂浮选流程半优先作业中的试验结果。试验结果表明 ,铜精矿品位提高 1 2 7个百分点 ,回收率 1 65个百分点 ,铜精矿中金和银的回收率分别提高7 43个百分点和 4 3
The test results of replacing OSN-43 # collector with PAC collector in half preferential flotation in Fenghuangshan Copper Mine's Concentrator are described. The tests showed the copper grade and recovery and the gold and silver recovery in the copper concentrate were improved by 1.27, 1.65, 7.43 and 4.33 percent points respectively.
出处
《金属矿山》
CAS
北大核心
2003年第3期30-32,共3页
Metal Mine