在常压条件下将珍珠岩尾砂进行湿法碱溶 ,碱溶液用水热合成法合成了 4A分子筛 ,采用正交实验确定了湿法碱溶及合成的工艺参数 ,经结构与性能验证合成的
In common pressure ,pearlite tailing is processed with wet process alkali dissolution method,the 4A molecular sieve was synthesized with alkali solution by water-heat synthesis method. Technology parameter of wet process alkali dissolution and synthesis was fixed by cross test.From the structure and properties test, the 4A molecular was up to standard.