摘要 研究了W 11- 4油田A平台排海污水中H2 S、钢桩上附着生物状态以及白色沉积物对平台海域钢结构设施腐蚀与防护的影响 ,测定了H2 S的浓度、分布以及含H2 S海水的腐蚀特征 ,研究了各种附着生物和白色沉积物的状态及组成 .结果表明 ,H2 S主要集中在海面海流下方区域 ,并与海水流速密切相关 ,最大可能H2 S浓度低于 19mg/L ;白色沉积物为附着生物受硫化氢影响的生理分泌物 ,海水中的H2 In order to understand the effects of hydrogen sulfide and white deposit in discharged waste water from oil platform on the corrosion and protection of the steel structure of W11-4 oil platform,a study was made by collecting the water samples,analyzing the concentration and distribution of hydrogen sulfide in the samples and the composition of the white deposit in the sea around the platform,and investigating its impact on the corrosion behavior of carbon steel.The results indicate that hydrogen sulfide mainly concentrates in the region of the sea near the surface,with a maximum of 19 mg/L,and its concentration greatly depends on the sea flow.The white deposit is the secretion from the attached marine organisms on the platform structure.It is also clarified that hydrogen sulfide and white deposit have no impact on the corrosion and protection of the steel structure of the oil platform.
出处 《中国腐蚀与防护学报》 CAS CSCD 2003年第1期38-45,共8页 Journal of Chinese Society For Corrosion and Protection
关键词 油田污水 硫化氢 平台钢结构 腐蚀 防护 hydrogen sulfide,concentration distribution,offshore oil platform,corrosion
  • 相关文献

参考文献3

  • 1[1]Videm K, Kvarekval J. Corrosion of carbon steel in carbon dioxide saturated solutions containing small amounts of. hydrogen sulfide[J]. Corrosion, 1995, 5 1 (4): 260
  • 2[3]Otero T F. Chronoampermetric study of mild steel pitting in sodiumsulfide aqueous solution[ J ]. Corrosion, 1994, 50(8): 576
  • 3[5]Sridhar N, Schutt H U, Anderko A M, Lencka M , Dunn D S. Ef fects of water and gas compositions on the internal corrosion of gas pipelines[J]. Corrosion, 2001,57(3) :221

同被引文献12

  • 1张亦良,王晶,陕小平,李邦宪.CNG气瓶在不同H_2S浓度中的临界裂纹尺寸[J].中国腐蚀与防护学报,2005,25(5):285-290. 被引量:7
  • 2Garber R. Higher hardenability low alloy steels for H2S resistant oil country tubular[J]. Corrosion, 1983, 39(3): 83 - 91
  • 3NACE Standard RP0472. Methods and controls to prevent in - service environmental cracking of carbon steel weldments in corrosive petroleum refining environments[S]. 1987
  • 4Adam Mazur. Segregation bands' role in H2S cracking of steels[J]. Mater. Perf., 1995, 34(7):52 - 54
  • 5Maria Sozanka, Jaroslav Sojka, Petra Bet'dkova, et al. Examination of hydrogen interaction in carbon steel by means of quantitative microstructure and fracture descriptions [J]. Mate. Charact.,2001, 46:239 - 241
  • 6Snape E. Sulfide stress corrosion cracking of some medium and low alloy steel[J]. Corrosion, 1967, 23(6): 154 - 172
  • 7Albarran J L, Martinez L, Lopez H F. Effect of heat treatment on the stress corrosion resistance of microalloyed pipeline steel [J].Corros. Sci., 1999, 41: 1037-1049
  • 8Merick R D. Refinery experience with cracking in wet H2S environment[J]. Mater. Perf., 1988, 27(1):30 - 36
  • 9Cantwen J E. LPG storage vessel cracking experience[J]. Mater.Perf., 1988, 27(10):79 - 82
  • 10Trivedi D K, Gupta S C. Cracking in liquid petroleum gas Horton spheres[J]. Mater. Perf., 1997, 36(7): 59 - 61

引证文献1

二级引证文献2

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部