摘要 热轧带肋钢筋的力学性能随时间变化而变化的特点使得企业检验出的力学性能与用户检验出的存在差异。为找出热轧带肋钢筋不同时间段力学性能的变化特点,对热轧带肋钢筋不同时间段的力学性能进行了试验。结果表明:10d(天)内热轧带肋钢筋的各项力学性能指标变化最快,20d后各项力学性能指标趋于稳定;其变化规律为屈服强度降低,抗拉强度、断后伸长率、最大力下总伸长率升高;屈服强度降低最多为17.31MPa,建议企业制定内控标准时屈服强度应比国标高20MPa。 The mechanical properties of hot rolled ribbed steel bars change with time,which makes the mechanical properties tested by manufacturer different from those tested by consumers.In order to find out the change characteristics of mechanical properties of hot rolled ribbed steel bars in different time periods,the mechanical properties of hot rolled ribbed steel bars in different time periods were tested.The results show that the mechanical properties of hot rolled ribbed steel bars changed rapidly within 10 d(days),and tend to be stable after20 d.The change rule is that the yield strength decreased,the tensile strength,the elongation after breaking and the total elongation under maximum force increased.The yield strength decreased by 17.31 MPa at most.It is suggested that the yield strength should be 20 MPa higher than GB when enterprises formulate internal control standard.
作者 杨凯 刘静 YANG Kai;LIU Jing(Shaanxi Steel Group Hanzhong Iron and Steel Co.,Ltd.,Mianxian 724200,China)
出处 《理化检验(物理分册)》 CAS 2019年第3期165-168,共4页 Physical Testing and Chemical Analysis(Part A:Physical Testing)
关键词 热轧带肋钢筋 力学性能 检验差异 内控标准 hot rolled ribbed steel bar mechanical property test difference internal control standard
  • 相关文献

参考文献8

二级参考文献18

共引文献64

同被引文献11

引证文献1

二级引证文献1

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部