提高150t炼钢系统板坯钢包自开率的实践

Practice on Improving the Automatic Casting Rate of Ladle of 150 t Steelmaking System
下载PDF
导出
摘要 围绕钢包水口座砖区域火山口形成原因,查找影响柳钢新150 t炼钢系统板坯钢包自开率低的原因,通过提高钢水洁净度、优化钢包顶渣、优化钢包流场、优化生产组织,使自开率由92.05%提高到96.49%。 The causes of low automatic casting rate of ladle of new 150 t steelmaking system were searched according to the reasons of crater forming in the nozzle pocket brick area.The automatic casting rate can be improved from 92.05% to 96.49% by enhancing the steel cleanliness,optimizing the top-slag of the ladle and the flow field of the ladle as well as the production organization.
出处 《柳钢科技》 2014年第5期22-24,共3页
关键词 板坯连铸 钢包 自开率 水口座砖 钢水洁净度 顶渣 流场 Continuous Slab Casting Ladle Automatic Casting Rate Nozzle Pocket Brick Steel Cleanliness Top-slag Flow Field