针对 6 A0 2 T6合金大断面型材在生产中时常出现性能波动的问题 ,本文着重从挤压工艺和热处理工艺两方面进行试验 ,提出了稳定 6 A 0 2 T6大断面型材性能的方法。
In view of performance fluctuation often occurred during the production of large section profile for 6A02T6,it was experimented on extruding process and heat treatment process in the article The way of stabilizing the property of large section profiles for 6A02T6 was also put forward