期刊文献+

负载型Au/CdOCO低温催化氧化性能的研究 被引量:2

Performance for Co Low-Temperature Oxidation Over Au/CdO Catalyst
下载PDF
导出
摘要 用共沉淀法制备了负载型Au/CdO催化剂。考察了以氧化镉为载体金催化剂的制备条件及CO低温催化氧化活性。结果表明,焙烧温度、预处理条件对催化剂的活性有较大的影响,573K焙烧,空气预处理的催化剂活性最好。XRD、TPR、TPD结果表明,活性金高度分散在氧化镉载体上,氧化态的金是活性中心,CO和O2均吸附在金上,其反应遵循Langmuir_Hinshelwood吸附机理。 Supported Au/CdO catalyst was prepared by co_precipitation.The preparation conditions and low_temperature catalytic activity for CO oxidation were studied.The results indicate that the activity of the catalyst is greatly related with the calcined temperature and the pretreatment condition.The highest activity is attained by calcination in 573 K and pretreatment in air.Results of XRD,TPR and TPD have showed that the active state gold disperses highly on CdO and catalytic active centers are the oxidized state gold.O2 and CO are adsorbed by active centers of gold.The reaction follows the Langmuir_Hinshelwood adsorption mechanism.
出处 《江西科学》 2003年第2期80-83,共4页 Jiangxi Science
  • 相关文献

参考文献14

  • 1王桂英,李雪梅,白妮,张文祥,蒋大振,吴通好.Au/ZnO催化剂的制备及常温常湿条件下CO氧化催化性能[J].高等学校化学学报,2001,22(3):432-434. 被引量:15
  • 2郝郑平,安立敦,王弘立.负载型金催化剂催化CO氧化的性能(Ⅱ)[J].分子催化,1998,12(1):63-66. 被引量:7
  • 3Haruta M,Yamada N, Kobayashi T,et al.Gold catalysts prepared by co-precipitation for low-temperature oxidation of hydrogen and of carbon monoxide[J] .J Catal, 1989,115:301 - 309.
  • 4Haruta M,Tsubota S, Kobayashi T, et al. Low-Temperature oxidation of CO over gold supported on TiO2,α-Fe2O3 and Co3O4[ J] .J Catal, 1993,144:175 - 192.
  • 5Tripathi A K, Kamble V S, Guota N M. Microcalorimetry Adsorption and Reaction Studies of CO,O2 and CO+O2 over Fe2O3,Au/Fe2O3 and ploycrystalline Gold catalysts as a Function of Reduction Treatment[J] .J Carol, 1999,187:332 - 342.
  • 6Wang Gui ying,Lian Hong Lei,Zhang Wen xiang.Stability and deactivation of Au/Fe2O3 catalysts for CO oxidation at ambient temperature and moisture[J]. Kinetics and Catalysis,2002,43:443 - 442.
  • 7Anguelina P K, Alexander I K,Sho Sugiyama, et al. Study of Gold species in Iron-Oxide-Supported Gold catalyt Derived from Gold-Phosphate Complex Au(pph3) NO3 and AS-precipitated wet Fe(OH)3 [J]. J Catal,1999,181 : 37-48.
  • 8Haruta M.Size-and Support-Dependency in the Catlysis gold [J].Catal Today, 1997,36:153 - 156.
  • 9Cunningham D A, Vogel H W. Torres Sanchez R M, et al. Structural analysis of Au/TiO2 Catalysts by debye function analysis[J] .J Catal, 1999,183:24- 31.
  • 10Hao Zheng ping, An Li dun, Wang Hong li, et al. Mechanism of gold activation supported gold catalysts for CO oxidation[J]. React Kinetic Catal Lett, 2000, 70: 153-160.

二级参考文献5

共引文献20

同被引文献50

引证文献2

二级引证文献9

相关作者