摘要
Molybdenum (VI) complex, namely molybdenum dioxobis(2,4-pentanedione) [MoO2(acac)2] used as epoxidation catalyst species, was synthesized and characterized by elemental analysis and infrared spectrum. Polystyrene-supported molybdenum dioxobis(2,4-pentanedione) [MoO2(acac)2] for synthesis of epoxycyclohexane was prepared by phase transfer catalysis method. Effects of various factors in synthesis of epoxycyclohexane by reaction of cyclohexene and t-BuOOH in the atmosphere of nitrogen catalyzed by polystyrene-supported MoO2(acac)2 were also investigated. Under the following conditions, n(cyclohexene):n(t-BuOOH)=3.5:l (based on 0.1 mol of t-BuOOH), volume of solvent -10ml, reaction temperature -80℃, reaction time -60min, and mass of molybdenum in the catalyst -2.30×0^(-3)g, the yield of epoxycyclohexane on the basis of t-BuOOH is over 99.5%, and the purity of epoxycyclohexane is about 99.9% by gas chromatogram(GC) analysis.
Molybdenum (VI) complex, namely molybdenum dioxobis(2,4-pentanedione) [MoO2(acac)2] used as epoxidation catalyst species, was synthesized and characterized by elemental analysis and infrared spectrum.Polystyrene-supported molybdenum dioxobis(2,4-pentanedione) [MoO2(acac)2] for synthesis of epoxycyclohexane was prepared by phase transfer catalysis method. Effects of various factors in synthesis of epoxycyclohexane by reaction of cyclohexene and t-BuOOH in the atmosphere of nitrogen catalyzed by polystyrene-supported MoO2 (acac)2 were aLso investigated. Under the following conditions, n(cyclohexene):n(t-BuOOH)=3.5:l (based on 0.1 mol of t-BuOOH), volume of solvent ~10 ml, reaction temperature ~80℃, reaction time ~60 min, and mass of molybdenum in the catalyst ~ 2.30 × 10^-3 g, the yield of epoxycyclohexane on the basis of t-BuOOH is over 99.5%, and the purity of epoxycyclohexane is about 99.9% by gas chromatogram(GC )analysis.
基金
Supported by the Outstanding Personality Innovation Funds of Henan Province(No.0121001900).