本文探讨了 1 0 6kA上插槽侧部炭砖破损严重的原因 ,总结了降低电流、降低效应系数等措施 ,可有效改善侧部炭砖的破损度 。
The paper discusses 160kA SSVC severely damaged cau se, sums up the measures of reducing the current strength and anode effect coefficient which improve the working life and reducing leakage of the cell in the side wall.
出处
《有色冶金节能》
2003年第3期52-54,共3页
Energy Saving of Nonferrous Metallurgy
关键词
铝电解槽
侧部炭砖
破损
改善措施
SSVC
side wall carbon block
damaged cause
improvement measure