6HAMMER T A.High strength LWA concrete with silica fume-ef- fect of water content in the LWA on mechanical properties,Sup- plementary Papers in the 4th CANMET/ACI Int.Conf.On Fly Ash, Silica Fume,Slag and natural Pozzolans in Concrete,Turkey, 1992 : 314-330.
7LURA P.Autogenous deformation and internal curing of concrete[C]. Ph.D.Thesis,Delft University of Technology,Delft,The Nether- lands, April 2003, ISBN 90-407-2404-0, 180.
9CUSSON D, HOOGEVEEN T.Internal curing of high-performance concrete with pre-soaked fine lightweight aggregate for prevention of autogenous shrinkage craekin[J].Conerete and Cement Cesearch, 2008(38) :757-765.
10JOSEPH G,RAMAMURTHY K,ASCE M.Autogenous curing of cold-bonded fly-ash-aggregate concrete[J].Journal of Materials in Civil Engineering, 2011,23 (4).