Φ4.6m×(9.5+3.5)m中卸原料磨裂纹故障的处理

Crack fault treatment of Φ4.6m×(9.5+3.5)m double rotator raw material mill
下载PDF
导出
摘要 江苏新街南方水泥公司2台Φ4.6 m×(9.5+3.5)m双滑履中卸四仓原料磨,在运行4年后在滑履带支承板及端头盖板等处出现多条裂缝。全面介绍了这2台原料磨裂缝的具体情况和原因分析;在此基础上,进行了维修方案的分析与评审;最后,就裂缝的具体修复过程及其实施效果进行了详细交流。此外,强调对关键设备(特别是大型设备的关键部位)的检查力度,做到定检和记录,以防止重特大事故的发生。 After four years of running, the two Φ 4.6 m ×(9.5+3.5) m double-slide-shoe four-chamber raw mills of Jiangsu XinJie Southern Cement Company have several cracks in the sliding track support plate and an end cover plate. State and causes of the cracks were introduced comprehensively, on this basis, analysis and review of the repair scheme were carried out. Finally, the concrete crack repair process and its implementation effect was communicated in detail. In addition, checks of the key equipment(especially the key parts of large equipment) and regular record to prevent serious accidents were stressed.
作者 冯海军
出处 《水泥工程》 CAS 2014年第1期50-53,共4页 Cement Engineering
关键词 中卸原料磨 滑履带支承板 端头盖板 裂缝 修复 跳动值 double rotator raw material mill slide-shoe support plate end cover plate cracks renovation beat value
  • 相关文献

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部