摘要
介绍了环氧彩色防滑路面材料固化机理以及在施工过程中出现的表层脱落、固化时间较长、气泡缺陷、泛白等主要问题,同时针对不同问题提出相应的技术及工艺对策,为环氧彩色防滑路面、环氧地坪施工均具有借鉴意义。
This paper introduced the curing mechanism of epoxy colored anti-slip pavement materials and the main problems of surface shedding, longer curing time, bubble defects, bleached etc. appeared in the construction process. At the same time, for the different problems, it also put forward the corresponding technical and technological countermeasures, which had reference value for the epoxy colored anti-slip pavement and epoxy floor construction.
出处
《山西交通科技》
2016年第2期16-18,共3页
Shanxi Science & Technology of Transportation
关键词
环氧
防滑路面
问题
对策
epoxy
anti-slip pavement
problem
countermeasure