4[1]Merhar J R. Overview of metal injection moulding[J]. Metal Powder Report,1990,45(5):339-342.
5[3]Ieki T, Katoh K, Matsumoto A, et al. Tensile properties of sintered Ti compacts by MIM process [J]. Journal of the Japan of Powder and Powder Metallurgy,1997, 44(5): 448-452.
6[4]Kato K, Katoh K, Ieki T. Tensile properties at high temperature of sintered TiAl compacts by MIM [J]. Journal of the Japan of Powder and Powder Metallurgy,1997, 44(11): 1029-1034.
7[5]Takekawa J, Sakurai N. Effect of processing condictions on density, strength and microstructure of Ti-12Mo alloy fabricated by PIM process [J]. Journal of the Japan of Powder and Powder Metallurgy, 1999, 46(8): 877-881.
8[6]Kaneko Y, Ameyama K, Sakaguchi S. Application of IM to Ti-5wt%Co and Ti-6wt%Al-4wt%V mixed powder [J].Journal of the Japan of Powder and Powder Metallurgy, 1990, 37 (5): 605-609.
9李惠萍译.用注射成形法制造钛合金鞋钉[J].钛合金信息,1995,(5):25.
10[8]Froes F H, German R M. Cost reduction prime Ti PIM for growth [J]. Metal Powder Report,2000,55(6) :12-19.