摘要
本文研究了H-13(4Cr5MoV1Si)钢的球化退火工艺。试验结果表明(870℃,2h+700℃,4h)等温退火是最佳的球化退火工艺。
This paper deals with the research work on the spheroidization annealing of H-13 (4Cr5MoV1Si) steel. The experimental results show that the isothermal annealing (870℃, 2 hours+700℃, 4 hours) is an optimum spheroidization annealing process.
出处
《上海金属》
CAS
1992年第2期42-45,共4页
Shanghai Metals