摘要 研究巨型工程机械子午线轮胎的变温硫化工艺。结果表明:与传统硫化工艺相比,采用变温硫化工艺(加热时间/保压时间比为1/1. 07)的巨型工程机械子午线轮胎胶料过硫化程度降低,物理性能提高;变温硫化工艺能提高巨型工程机械子午线轮胎硫化均匀性,解决局部过硫严重的问题;采用变温硫化工艺,调整加热时间与保压时间比,有利于提高巨型工程机械子午线轮胎性能和生产效率,节约能源。 Non-isothermal curing process of giant OTR radial tire was studied. The results showed that,compared with the traditional curing process,giant OTR radial tire cured with non-isothermal process(heating time/dwell time ratio was 1/1. 07) had a lower degree of over curing and better physical properties,nonisothermal curing process could improve vulcanization uniformity and solve the problem that some parts were over cured seriously. By adjusting the heating time/dwell time ratio during non-isothermal curing process,properties and production efficiency of giant OTR radial tire were improved,and the energy consumption of the production process was reduced.
作者 武栴丞 李文东 杨茂林 曾季 蔡庆 黄振华 施大全 WU Zhancheng;LI Wendong;YANG Maolin;ZENG Ji;CAI Qing;HUANG Zhenhua;SHI Daquan(Beijing Research & Design Instiute of Rubber Industry Co.Ltd,Beijing 100143,China;Fujian Haian Rubber Co.Ltd,Putian 351100,China)
出处 《橡胶工业》 CAS 2019年第2期142-145,共4页 China Rubber Industry
关键词 巨型工程机械子午线轮胎 变温硫化 过硫化程度 硫化均匀性 giant OTR radial tire non-isothermal curing degree of over cure vulcanization uniformity
  • 相关文献

参考文献2

二级参考文献4

  • 1王伟,邓涛,赵树高.轮胎硫化工艺条件的优化[J].轮胎工业,2006,26(4):225-227. 被引量:8
  • 2三角轮胎股份有限公司,北京化工大学.轮胎直压成型电磁感应加热硫化方法及其专用内模[P].中国:CN103286893A,2013-09-11.
  • 3Eckert E R G, Drake R M. Analysis of Heat and Mass Transfer[M]. NewYork: McGraw Hill, 1972 : 1 49.
  • 4杨其,王海,冯彦龙,李可萌,苏巨桥,吴世见.橡胶轮胎硫化测温技术[J].轮胎工业,2008,28(8):496-499. 被引量:4

共引文献5

同被引文献76

引证文献23

二级引证文献33

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部