粉末布法制备SiC/Ti基复合材料 被引量:5

Preparation of SiC/Ti composites by powder cloth technique
下载PDF
导出
摘要 用粉末布法制备了低成本SiC/Ti基复合材料。结果表明,采用合适的轧制参数即可容易地获得厚度合适、均匀的粉末布;热失重分析和热解残余物分析指出用来制备粉末布的有机粘结剂的去除过程分成两个阶段,合理除气后,基本没有残余物。使用真空热压工艺制备的SiC/Ti基复合材料,纤维分布基本均匀,纤维与基体的界面结合良好。 The low cost SiC/Ti composites were prepared by a powder cloth technique. It is shown that uniform powder cloth with proper thickness can be produced by using appropriate rolling parameters. Thermogravimetic and pyrolysis residuum analysis indicate that the burnout process of fugitive binder used to produce the cloth is found to take place in two stages, no residuum is left when degassed properly. Composite materials processed by the vacuum hot pressing exhibit uniform fibre distribution and high interface bonding strength.
出处 《中国有色金属学报》 EI CAS CSCD 北大核心 2004年第3期465-470,共6页 The Chinese Journal of Nonferrous Metals
基金 中国科学院"百人计划"项目
关键词 SiC/Ti基复合材料 粉末布 制备 SIC纤维 真空热压 titanium matrix composite powder cloth SiC fibre vacuum hot pressing
  • 相关文献

参考文献11

  • 1[1]Guo Z X, Derby B. Solid-state fabrication and interfaces of fibre reinforced metal matrix composites[J].Prog Mater Sci, 1995, 39(4 - 5): 411 - 455.
  • 2[2]Guo Z X. Towards cost effective manufacturing of Ti/SiC fibre composites and components [J]. Mater Sci Tech, 1998, 14(Sep-Oct ): 864-872.
  • 3[4]Mackay R A, Brindley P K, Froes F H. Continuous fibre-reinforced titanium aluminide composites[J].JOM, 1991(5): 23-29.
  • 4[5]Brindley P K, Draper S L, Eldridge J I, et al. The effect of temperature on the deformation and fracture of SiC/Ti-24Al-11Nb[J]. Metall Mater Trans A,1992, 23A.. 2527-2540.
  • 5[7]SHI Z, GUO Z X, SONG J H. Kinetic modeling of binder burnout for optimization of slurry-powder manufacturing process of Ti/SiC composites[J]. Mater Sci Tech, 2000. 16(7 - 8): 843 - 847.
  • 6[10]SHI Z, GUO Z X, SONG J H. A diffusion-controlled kinetic model for binder burnout in a powder compact[J]. Acta Mater, 2002, 50: 1937- 1950.
  • 7[11]Baumann S F, Brindley P K, Smith S D. Reaction zone microstructure in a Ti33Al+ Nb/SiC composites[J]. Metall Mater Trans A, 1990, 21A: 1559 -1568.
  • 8[12]Thomas M P, Winstone M R. Longitudinal yielding behaviour of SiC fibre reinforced titanium matrix composites[J]. Comp Sci Tech, 1999, 59: 297-303.
  • 9[13]Peng H X, Dunne F P E, et al. Fibre re-arrangement and matrix softening phenomena in matrix-coated fibre(MCF) composites during vacuum hot pressing consolidation[J]. Mater Sci Eng A, 2003, A346:246 - 253.
  • 10[14]Baik K H, Grant P S. Strength degradation of SiC fibre during manufacture of titanium matrix composites by plasma spraying and hot pressing[J]. Metall Mater Trans A, 2001, 32A: 3133-3142.

同被引文献46

引证文献5

二级引证文献7

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部